SMT / Soldering Lee Whiteman, PMP Senior Member Engineering Staff L-3 Communications East Telephone: (856) 338-3508 FAX: (856) 338-2906 E-Mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick Sent: Thursday, April 23, 2009 3:50 PM To: [log in to unmask] Subject: Re: [TN] Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) Lee, Wire bonding or SMT/soldering? My assumption is the latter, but thought I would ask anyway. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman Sent: Thursday, April 23, 2009 2:11 PM To: [log in to unmask] Subject: [TN] Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) Does anyone have any opinions of using Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) as a board finish for high reliability aerospace applications? You can contact me off line if necessary... Thanks again. Lee Whiteman, PMP Senior Member Engineering Staff L-3 Communications East Telephone: (856) 338-3508 FAX: (856) 338-2906 E-Mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------