No issues. It was qualified as a conformal coating rework solution. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson Sent: Thursday, April 02, 2009 8:39 AM To: [log in to unmask] Subject: Re: [TN] Solvent for cured cyanoacrylate adhesive >>> It does an excellent job of cleaning TakPak, Loctite 3621, 3609, 3607 and other epoxies And so you need to ask what underlying substrate the adhesive is on - anything which will clean epoxies is likely to dissolve/damage most pcb's and components, for example. Regards, Peter -------------------------------------------------------- Peter Swanson [log in to unmask] INTERTRONICS http://www.intertronics.co.uk Tel: +44 1865 842842 Oxfordshire, England INTERTRONICS is dedicated to providing quality material, consumable and equipment solutions to the high technology, high performance assembly industries, incorporating outstanding levels of technical support and customer service. Read our news! http://www.intertronics.co.uk/blog/blog.htm INTERTRONICS is the trading name of Cygnet Electronics Ltd, registered in England No 1835617. Registered office: 17 Station Field Industrial Estate, KIDLINGTON, Oxfordshire, OX5 1JD, ENGLAND. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: 02 April 2009 14:29 To: [log in to unmask] Subject: Re: [TN] Solvent for cured cyanoacrylate adhesive Steve, I have used conformal coat thinner that is about 80% MEK. It does an excellent job of cleaning TakPak, Loctite 3621, 3609, 3607 and other epoxies. Try that first. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Thursday, April 02, 2009 8:09 AM To: [log in to unmask] Subject: [TN] Solvent for cured cyanoacrylate adhesive Mornin' all, I have a question for the chemists out there about the solvent used to clean-up cured cyanoacrylate adhesives. Loctite sells a solvent called 768 X-NMS Solvent that works pretty well, but it is expensive. Anywhere from $20.00 to $37.00 for a little 1.75 ounce bottle depending on where you buy it. I do know that it is composed mainly of nitromethane with a little bit of toluene according to the MSDS. My question is; I can get a gallon of nitromethane at a high-performance auto parts store store nearby for $50.00 a gallon, would pure nitromethane do the job? Or do I need to add the toluene as well? The MSDS gives a range of percentages of both components, but is kind of vague: http://www.rshughes.com/images/products/docs/zwNFyUtpQskOxsrawO1uew.pdf I'm just trying to save a little money is all... Steve --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------