van der Waals Bev -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Sent: Friday, April 10, 2009 4:19 PM To: [log in to unmask] Subject: Re: [TN] Friday Theorizing It's an interesting question. You need know what 'adhesion' means in a deeper meaning. Ask an adhesive specialist and he will give you a whole bunch of explanations, like chemical bonds, atomic bonds, van de Vaals bindings (not sure I spell it correctly), electrostatic bindings, mechanical bindings etc. The little I've understood gives, that an essential part of bindings in fact are mechanical. Depending on the viscosity of the epoxy and its wetting characteristics, the micro roughness is important. Hence, the tin process (and the copper etching) ought to be such that you get as much porosity as possible. It reminds of thickfilm technology in a way. Here, mechanical binding are a big percentage of the binding, besides the oxide binding. One way to 'roughen' the tin could be a second or two etching. I've studied the result in a SEM. The difference between the etched and non etched tin is obvious. I realize that performing such a treatment on a one micron tin layer is not to be done by others than experts. Will be interesting to see what Rudy Sedlak and like will add as professionals. And finally I wonder how the epoxy process will be done without voids and gas bubbles. Vacuum oven? Here is a good paper that explains in detail. http://www.sjsu.edu/faculty/selvaduray/page/papers/mate210/interfacial.pdf Inge ----- Original Message ----- From: "bob wettermann" <[log in to unmask]> To: <[log in to unmask]> Sent: Friday, April 10, 2009 5:16 PM Subject: Re: [TN] Friday Theorizing > Thanks all to have responded. > > More options came up yesterday in speaking with other suppliers of the 1oz > base copper material. There are versions which have : > > 1. 8-10 microns roughness on one side (this will be electroplated with > 1-1.4 microns of tin) > > 2. 0.3-0.4 microns roughness on the other side (this too will be > electroplated with 1-1.4 microns of tin) > > So now my question for you metalurgists out there is the same .....if I > bond at room temp for room temp use using a 2-part epoxy SIDE 1 described > above to the FR4 should I expect adequate adhesive strength (compared to a > 1oz copper trace/pad run through an initial mfg process)? > > Happy Easter > > Bob Wettermann > PH 847-767-5745 > > > > > ________________________________ > From: Richard Stadem <[log in to unmask]> > To: [log in to unmask] > Sent: Friday, April 10, 2009 8:58:26 AM > Subject: Re: [TN] Friday Theorizing > > As I stated in my earlier posting, there are certain epoxies that bond > well to > tin-plated copper. One that I described was pull-tested to 18 lbs before > it > pulled the foil away from the PWB. On the side where the same epoxy was > used to bond the plated foil to the PWB, parts of the FR-4 substrate came > up > with it. > Of course, this has to be done after reflow. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------