Denny, Steve, Dave, et al Thanks for all the feedback. I knew, of course, about tin and had heard some things about cadmium years ago but dismissed them because cadmium use was declining for much of everything but government spec'd corrosion requirements. Curious if the zinc whisker propensity is more or less for electroplated vs. galvanized zinc. Anyone know? Roger --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------