In a previous life I use to do a lot of pull tests and usually the wires would break before the crimping area. So I agree that the problem may be over-crimping. I also use to test the strength of the wires alone, without crimps. It was a reliable way to know if the crimps were good. If the crimped test were way below single wire (if the wires broke and not pulled off of course) I knew we had problems of over crimping. Jean-François Bissonnette t : 450-967-7100 ext : 242 [log in to unmask] www.digico.cc P N'imprimer que si nécessaire - Print only if you must -----Message d'origine----- De : Temkin, Gregg [mailto:[log in to unmask]] Envoyé : 11 mars 2009 11:24 À : [log in to unmask] Objet : Re: [TN] Cable Pull Test specifications Actually too tight a crimp is often the cause of such failures. The Circular Mil Area of many high count stranded wires is often greater than that of its solid or low strand count equivalent. Suggest you have them verify they're not over-crimping, and, if their tool is adjustable, see if they can back it off a little. Gregg -----Original Message----- From: Forrester, Michael (H USA) [mailto:[log in to unmask]] Sent: Wednesday, March 11, 2009 7:00 AM To: [log in to unmask] Subject: [TN] Cable Pull Test specifications I have a cable vendor that states the following: "Currently have issue with inconsistency of tensile strength of the crimp using wire ULTRA-FLEX PVC 1251/14 BLACK, due to the flexibility of this wire item and the large amount of strands, at 1050 strands at 44AWG. After conducting several pull tests found that the breaking points all ranged from 44lbs to 49 lbs with no consistency. I then conducted a pull test on a typical 14 AWG, 19 strand wire and the result was 89 lbs for comparison purposes. Due to not being able to duplicate the acceptable pull test from previous shipments and considering the properties of this high stranded and flexible wire we feel it will not consistently meet the UL 486 standard 14 AWG pull test requirement of 50lbs" During testing, the cable breaks right at the crimp. Should the cable be able to take the 50 lbs even though there are many fine strands making up the 14 AWG wire? Is the cable not crimped properly and only the outer strands are taking the load cusing a "failure". The vendor is looking for a deviation to reduce the pull test requirement to 45 lbs. Since the Mil-T-7928 spec is 70 lbs and the UL 486 spec is 50lbs, I'm not sure if the make-up of the wire (fine strands) really factors in or the vendor needs to crimp tighter on the cable to add strength? Any comments would be welcomed. Thank you. Michael Forrester Sr. Product Engineer Siemens Healthcare Diagnostics 101 Silvermine Rd. Brookfield, CT 06804 PH: (203) 740-6452 The attachment named could not be scanned for viruses because it is a password protected file. ---------------------------------------------------------------------------- This message and any included attachments are from Siemens Medical Solutions and are intended only for the addressee(s). The information contained herein may include trade secrets or privileged or otherwise confidential information. Unauthorized review, forwarding, printing, copying, distributing, or using such information is strictly prohibited and may be unlawful. If you received this message in error, or have reason to believe you are not authorized to receive it, please promptly delete this message and notify the sender by e-mail with a copy to [log in to unmask] Thank you --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------