You are probably going to be physically limited to 3/8th of an inch (0.375, 10mm). Most likely the wave dynamics to accomplish this will create a lot of dross. Dewey -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea Sent: Tuesday, March 10, 2009 11:46 AM To: [log in to unmask] Subject: [TN] Max height of components acceptable for wave pallets Dear Technos, What is the maximum height of the components on the solder side that will allow for using wave soldering masking fixtures? Thank you, Ioan Tempea, ing. Ingénieur Principal Fabrication / Sr. Manufacturing Engineer 30 ans déjà! - Already 30 years! 950 rue Bergar, Laval, Québec, H7L 5A1 t : 450-967-7100 ext : 244 Mtl : 514-990-5762 f : 450-967-7444 [log in to unmask] www.digico.cc <http://www.digico.cc/> P N'imprimer que si nécessaire - Print only if you must --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------