Jim, Chip resistors seldom fail cracked due to a simple structure and materials that have high modulus of elasticity. Ceramic capacitor are complex multi layer structures with a much lower modulus. Most ceramic caps are X5R/X7R and are made with barium which is an excellent x-ray absorber. Plus x-ray usually does not adequate to observe cracks. All one will observe are nick dark rectangles in the images. Acoustic microscopy could be used but depending on the chip size and location of tall parts it may not be practical as the assembly must be submerged in water while under test. The transducer needs to be physically close to the assembly surface precluding most fully populated assemblies from being scanned. Additionally most assembly cracks are located beneath the terminations that obscure definitive imaging while mounted on the assembly. Interesting problems with not many solutions. Regards, John Maxwell ----- Original Message ----- From: "Jim West" <[log in to unmask]> To: <[log in to unmask]> Sent: Monday, March 09, 2009 4:28 PM Subject: [TN] Detection of potential cracked capacitors and resistors Looking for a quick/easy way (if this is even possible), to verify if ceramic capacitors and/or resistors placed on a PCA are cracked. Can an X-ray be used to check for cracked capacitors and resistors? We had an issue with hand soldering of other components that compromised the PCA and could possibly lead to cracked components. If X-ray cannot detect the cracks, are they other methods of inspecting for cracked components that you guys can think of? Besides electrical test (PCA's will not fit in electrical test fixture now due to hand mounted components). Thanks, Jim --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------