Wirebonding setup is often painful. Using "setup parts" which weren't made at the same fabricator as the parts you are planning to use is only helpful for training on the machinery. Gold plated (over nickel of course) Kovar about 0.5mm thick welds (wirebonds) readily and is pretty easy to get. So I recommend that for training purposes. If you REALLY want to play with semiconductor die, then I'd recommend calling ChipSupply or one of the other die distributors to see if they care to unload junk parts. But they could be junk because they have too small a parameter "window" for production wirebonding, so you could just be learning how difficult things can be by getting them. Wayne Thayer ________________________________________ From: TechNet [[log in to unmask]] On Behalf Of bob wettermann [[log in to unmask]] Sent: Thursday, February 26, 2009 10:03 AM To: [log in to unmask] Subject: [TN] Wire Bonding Dummy Parts Dear Technetters: Anyone know of a vendor of dummy parts for gold wire signal bonding for practicing? Regards Bob Wettermann PH 847-767-5745 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------