Denny, There has never been a case of lead fumes in any normal soldering process - the temperatures are too low. In my lead pollution presentation I have added in a slide that compares the vapor pressure of mercury to that of lead. The difference is quite stark. There is no currently available reasonable method that I know of to detect the infinitesimal amount of elemental vaporized lead over a soldering iron or solder pot set at any temperature that would ever be seen by a circuit pack during manufacturing or rework. It is a different story regarding lead oxide negligently drossed off of a wave solder pot. Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad Sent: Tuesday, February 17, 2009 12:25 PM To: [log in to unmask] Subject: Re: [TN] Leadfree has gone too far. Hi Denny We need Cr3 in our diets as an aid in glucose metabolism, the same case, cannot be made for lead. As for the lead industry lack or response, with lead in solder representing less than 0.5% of all lead used annually, there was not enough there to for them to worry about, on the other hand the increased use of tin was very beneficial to that industry and would provide ample incentive to have lead in solder blackballed, whether or not they actually ever did so is known only for certain by the leaders of tin industry. ( with the word leaders obviously pronounced "leeders" not "leders"... ;-) Cheers, Joe In a message dated 2/17/2009 8:30:57 A.M. Pacific Standard Time, DDFRITZ writes: My ancient chemical engineering degree stirs me to comment on this thread (always dangerous) The main culprit in lead uptake by all animals is the chemistry of the lead. Oxidized state lead - lead oxide left from burning leaded gasoline, or lead chromate from the various yellow, orange and red lead pigments in paints is very easy for the blood to pick up. Tetraethyl lead for leaded gas is horribly toxic to all animals because it is so very easy to absorb (remember washing grease off your hands with gasoline before about 1970?). That ionized lead is still out there in the paint chips or soil surface layer, as Joe points out. Elemental lead is pretty innocuous to animals (carrying a bullet from the war, etc.) except for one nice way to create ionic lead in the body - the stomach acid that works on elemental lead when eaten. That is not very fast, but it is steady - in the case where the lead remains in the stomach - ducks whose gizzards grind shot or sinkers against sand and gravel in digestion, someone's cow where the weight stayed at the bottom of one of the four stomachs, or sadly, some super cheap lead trinkets that lodged in small child stomachs or intestines. Don't forget the cheap yellow and orange paint on toys - we covered that before. I think years ago on TechNet, we discussed how much lead is absorbed from lead solder assembly - I can't remember a single case of significant lead fumes - am I wrong? Sanity says to ventilate - the flux smell can get to you. I hear about lead exposure from "roasting circuit boards on an open fire" in third world countries. How much of that is no hand washing instead of breathing? How much from using the same pot for stir fry as for roasting boards? How did we get the environmentalists to limit chrome controls to Chrome +6? A better marketing job by the "Chrome Industry Council"?. Lawmakers still wanted their shiny cars and plumbing fixtures? The stainless steel folks drove some sanity? Guess there is no "Lead Industry Council" to stand up for their product. My simple answer would be to restrict lead where it is ionic (done now through these bans), AND elemental lead where it can easily be ingested - shotgun shot, sadly for me fishing sinkers, and anything say smaller than 2 ounces. And, in my opinion, lead in solder for circuit boards is safe - who eats them? I think IPC helped get circuit boards in toys exempted from this legislation, right? What da ya think? Denny Fritz -----Original Message----- From: Joe Fjelstad <[log in to unmask]> To: [log in to unmask] Sent: Tue, 17 Feb 2009 10:49 am Subject: Re: [TN] Leadfree has gone too far. Unfortunately, the road to perdition is paved with good intentions and it's sad to say, but common sense is not so common anymore. I am confident that there are many folks out there paving the road who are applauding this news. So it goes... Joe PS Steve's observations are on target. The lead acetate (aka lead sugar) in paint is what make eating paint chips attractive to children. The elimination of lead from gasoline and paint were two of the best solutions to reducing lead in the environment. Others have followed wanting to build on that legacy using assertion without proof and conjecture rather that science or data. For the record, the discovery of the fall out from lead in gasoline came when there was a study done to see if there was risk from using tin-lead solder for canned food lids which was shown to account for a smaller percentage than expected. The "no effect" limit for lead consumption is 3 mg per person per week according to "Encyclopaedia of Environmental Agricultural Pollution and Its Control" By G.R. Chhatwal. in Chapter 21 "The Impact of Inorganic Spoil Pollutants on Consumers" (but it was not recommended ;-) He also pointed out lead paint licking by animals as one of the prime sources and reported in the book that higher calcium intake significantly reduced lead uptake/absorption. Interestingly, most of the lead comes from the soil attached to the roots eaten by grazing animals. Given the fact that a micro thin layer of lead has been deposited all over the land over for the half century that leaded gasoline was most common, it reinforces the validity of the ban (though it is still in use for some aviation fuel and in some less developed countries I believe) In a message dated 2/17/2009 6:12:25 A.M. Pacific Standard Time, [log in to unmask] (mailto:[log in to unmask]) writes: The kid in the picture might accidentally eat the battery terminals. I just had to laugh. _http://www.startribune.com/local/39693797.html?elr=KArksLckD8EQDUoaEyqy P_ (http://www.startribune.com/local/39693797.html?elr=KArksLckD8EQDUoaEyqy P) 4O:DW3ckUiD3aPc:_Yyc:aULPQL7PQLanchO7DiUss ____________________________________ A Good Credit Score is 700 or Above. _See yours in just 2 easy steps!_ (http://pr.atwola.com/promoclk/100126575x1218822736x1201267884/aol?redir =http://www. freecreditreport.com/pm/default.aspx?sc=668072&hmpgID=62&bcd=febemailfoo terNO6 2) **************You can't always choose whom you love, but you can choose how to find them. Start with AOL Personals. (http://personals.aol.com/?ncid=emlcntuslove00000002) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------