We have seen this a few times. There seem to be two reasons why: CTE mismatch Cu/Ni and brittle Nickel caused by excessive additives. Inge ----- Original Message ----- From: "Lee Whiteman" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, February 11, 2009 7:20 PM Subject: [TN] CRACKED ENIG PADS I have asked Steve to put up a pair of pictures I received. They are of cracks within the ENIG finish of a PWB. I know that the board failed, based on IPC-6011 and IPC-6012. My question is what would cause the cracking? Evidently, it is in the Nickel layer and the copper layer was not compromised. There was no evidence of a lack of bonding between the copper and the ENIG finish. These boards are fresh from the supplier. Just curious... Thanks in advance. Lee Whiteman, PMP Senior Member Engineering Staff L-3 Communications East Telephone: (856) 338-3508 FAX: (856) 338-2906 E-Mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------