Ingemar, In my mind the decision for air vs screw [air time-pressure vs positive displacement] is made on the basis of just how much volumetric control you require [and the characteristics of the material]. If the RT time vs viscosity characteristics of the material allow you to go with a simple time/pressure arrangement, then all you need to hang on the end of your robot arm is a syringe and needle. Cleanup is a snap. I hate cleaning the screw/auger systems!!! Things get even more complicated with short pot-life materials. It always seems like someone in production 'forgets' to clean the system before leaving for the weekend ... leading to cost and delay issues the following Monday. I would certainly try an experiment with time vs pressure first. If that doesn't work, well there are other positive displacement systems that are less cumbersome than the screws. Asymtek and others for example [$] Did I say that I like the old time vs pressure approach if I can get away with it?? :-) Best wishes Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Sent: Monday, February 09, 2009 3:54 PM To: [log in to unmask] Subject: [TN] robotic dispensing Hi all, have to buy or lease a 6axis robot for dispensing UV cured conductive epoxy in thousands of small tubes or channels. Strings 0.5 mm wide and 20 mm long. Only the dispenser tip can enter, the rest of the dispenser must stay outside the target. Speed is of no interest, quality the more. It's a very small one, only 500 pounds of weight and max payload 10 pounds. All DC motors, no hydraulics. Position accuracy is 50 micrometers. Q: anyone with opinion what is best, pressurized air piston or screw? Are there dispensers for easy robotic hand mount? Inge --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------