On 2 Feb 2009 at 8:59, Graham Collins wrote: > Hello Technet > I've got a design where we have to run a jumper between two adjacent > legs of a fine pitch part. So the jumper is a tiny piece of wire that > runs down the leg, across the foot, bends around in a U, and back up > the adjacent lead. We hand form this, and the operators are not > liking it. I'm pondering getting the machine shop to try to make > something we could use to pre-form the wire for this, but it's a bit > higher precision than they usually work to. The gap between component > leads is about .012" 12 mil, = 0,305mm. I assume no track between these pins? Is it allowed just to connect the two pins with a blob of solder? Maybe easier with just a short wire snippet squeezed in the gap between the pins, would make it easier to get this normally unwanted "solder defect". Don't know what any current versions of IPC-7721 or similar docs state about that modification. My version is about 10 years old, but the latest seems to be from 2001, still nothing about such fine pitch stuff in the latest addendum... Best regards Matthias Mansfeld -- Matthias Mansfeld Elektronik * Leiterplattenlayout Neithardtstr. 3, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8 Internet: http://www.mansfeld-elektronik.de GPG http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------