Assumming you do pattern plating and you are talking about full body hard gold.
Copper plate - Nickel/Gold flash - Etch - Solder Mask - Selective image - Hard gold plating on the fingers (be sure you have the bussing)
Some people do ENIG and gold fingers. Same thing using selective image for gold finger plating after solder mask. Best regards, Jason Zhao Dynamic Flex, LLC US 510-468-4412 China 137-74692180 --- On Wed, 1/14/09, lium <[log in to unmask]> wrote:
From: lium <[log in to unmask]> Subject: [TGAsia] 咨询 To: [log in to unmask] Date: Wednesday, January 14, 2009, 3:22 AM