Oops, second line should have been ID -----Original Message----- From: Temkin, Gregg [mailto:[log in to unmask]] Sent: Monday, January 26, 2009 7:10 AM To: [log in to unmask] Subject: Re: [TN] NAS620C4 The spec states: For OD the tolerance is +.015/-.005 For OD the tolerance is +.010/-.000 For thickness the tolerance is as stated in note 2 2. TOLERANCES: ALL WASHERS MUST BE FLAT WITHIN .007 INCH AND PARALLEL WITHIN .002 INCH. TOLERANCE ON THICKNESS "T" IS TO BE IN ACCORDANCE WITH THE SHEET TOLERANCE REQUIREMENTS OF THE APPLICABLE MATERIAL SPECIFICATION. For Stainless Steel, the material spec is ASTM A240. I don't have a copy of that spec handy. Gregg -----Original Message----- From: Mike Sewell [mailto:[log in to unmask]] Sent: Monday, January 26, 2009 6:34 AM To: [log in to unmask] Subject: [TN] NAS620C4 What are the tolerances for a NAS620C4 washer? I've got the nominal dimensions, but don't have access to the NAS620 spec... Thanks, Mike --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------