Hi All. My question is related to a comment one of our CMs recently made about not allowing populated/soldered boards to come in direct contact with pink colored antistatic foam for extended periods of time. This CM was notified by another customer that they observed discoloration of solder joints, solderability issues and /or conformal coat adhesion problems after ~ 90 days due probably to either out gassing and/or a chemical reaction with the ant-stat chemicals used in the foam. At one time I did hear about N'octonic acid (not sure of spelling) in pink poly static bags causing problems but have not heard anything recently. Has anyone heard of or experienced such issues with the use of such material as pink colored antistatic foam? Is there a safe anti-stat foam that does not have these issues/concerns? Is there a mil spec or some other industry type spec that regulates the type of anti-stat material used with electronics? thanks Best Regards, -Joe "This e-mail and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as U.S. Government export controlled technical data. If you are an unintended recipient of this e-mail, use, disclosure or distribution of its content is prohibited. Please notify the sender by return e-mail and immediately delete this message." --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------