Applying heat evenly to both sides helps prevent board warping. If the board is warped even a little during solder joint formation, when it cools the joints will be under stress and possibly lead to cracks, etc. Kevin Glidden Manufacturing Engineer Luminescent Systems Inc. -----Original Message----- From: Eli Sarig [mailto:[log in to unmask]] Sent: Tuesday, January 06, 2009 2:16 PM To: [log in to unmask] Subject: [TN] Question about bottom heaters of reflow oven Hi all, My question is related to the necessity of down heaters in the reflow oven. When we solder double sided boards, we *can* create a suitable reflow profile using *only* the top heaters of the oven. In that case, the bottom heaters remain at room temperature. We measure almost the same temperature on top and bottom of the board. Are there any limitations or problems that might happen using this kind of process? Thanks, Eli. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------