Dewey, What kinds of plastics or polymers are you talking about? Doug Pauls Rockwell Collins "Whittaker, Dewey (EHCOE)" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 01/28/2009 08:27 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Whittaker, Dewey (EHCOE)" <[log in to unmask]> To [log in to unmask] cc Subject [TN] Plastic I know a lot of you have had suspicions of this, but I am lost in the ozone again. I have a request for any test data on the compatibility and use of non-metals in a 1.2 PPM ozone environment at 35,000 to 50,000 ft.elevation. With all of the space constraints I have had to reduce all my old files on plastics, so I am starting from scratch again. It gives a whole new meaning to your knowledge of plastics starts to mold. TIA Dewey --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------