Hi Dave! My suspicion is that the pdb fab is proposing plating and then filling, followed by overplating. That way if breakout occurs on the final etch there will still be lots of plated contact to the escaping trace. I don't know if it makes Class 3--I suspect not. Trying to fill such a tiny through hole could be a problem if the board is thick. In any case, I prefer non-conductive via plugging material because the silver can create bad intermetallics at high temperatures--such as Pb-free reflow. Wayne Thayer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt Sent: Tuesday, December 02, 2008 10:01 AM To: [log in to unmask] Subject: Re: [TN] Conductive Epoxy filled Vias Joyce, Our board house is concerned about meeting the 0.003" annular ring requirement with a drill and hole size that small. Remember they have to use a larger drill size to get our finished hole size. The conductive epoxy sounds like it will "relieve us" of that issue.. Dave Connitt -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Tuesday, December 02, 2008 9:16 AM To: [log in to unmask] Subject: Re: [TN] Conductive Epoxy filled Vias Why not plated via? -------------------------- Sent using BlackBerry ----- Original Message ----- From: TechNet <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Sent: Tue Dec 02 09:07:27 2008 Subject: [TN] Conductive Epoxy filled Vias Hello List, We are considering implementing a 0.80 mm pitch BGA on a development project and I have question about escape vias. The part manufacturer recommends that we use a 0.019" pad with a 0.010" drill. The board has to be a IPC-6012 class 3 PWB and I would like to have a 0.003 annular ring on the escape vias. One of our board vendors suggested we use a epoxy filled via which would relieve us of the annular ring issue but I am not sure about still being a class 3 board. Does anybody know where I can confirm that epoxy filled vias are acceptable in a class 3 board? Thanks, Dave Connitt CID+ Printed Circuit Designer KDI Precision Products, Inc. A Wholly Owned Subsidiary of: L3 Communications 3975 McMann Road Cincinnati, Ohio 45245 Ph. 513- 943-2010 Fax 513-943-2288 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------