Technically if you apply liquid flux to a joint and apply a soldering iron to the joint you are doing the same thing... The difference is that there is less available free alcohol.. Alcohol is a polar enough to be a carrier for rosin but not really polar enough the act like a "real" solvent...It is a real solvent if you have a really long time to wait...The alcohol surrounds the rosin molecule groups which allows the rosin to be soluble in the alcohol...This is because the rosin has higher internal energy then the alcohol so it doesn't readily dissolve into the alcohol... When your soldering iron hits the flux it first flashes off the free alcohol then heats up the resin... That's one of the reasons old rosin fluxes or cored wire doesn't work as well as new liquid fluxs... Paul Paul Edwards -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Thursday, December 18, 2008 5:34 AM To: [log in to unmask] Subject: Re: [TN] flux and board cleaning issues And your fire marshall is OK with the concept of applying a hot soldering iron to a flammable solvent? I'd get shot if I suggested that here. Doug Pauls Rockwell Collins Paul Edwards <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 12/17/2008 08:32 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Paul Edwards <[log in to unmask]> To [log in to unmask] cc Subject Re: [TN] flux and board cleaning issues Andy, First you put on the alcohol and just start soldering.. Adding liquid flux and solder wire... First the alcohol coats the PCB with a micron-thick layer that prevents the flux residues from adhering to the PCB Then the violent boiling action of the alcohol, thermo-mechanically scrubs the joint areas of oxides and residues, transports the residues away from the joint area and then keeps the flux and residues from adhering to surfaces do to the solution movement ... For your own processes and chemicals you have to develop "recipe"... You sometimes end up using different alcohol percentages to insure you have a consistent H20 to alcohol ... Paul Paul Edwards -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Andy Ng Sent: Wednesday, December 17, 2008 6:09 PM To: [log in to unmask] Subject: Re: [TN] flux and board cleaning issues Paul, can you clarify on your statement "To make the NC flux easier to remove we normally put alcohol on soldering area before soldering with NC flux..." Did you mean to put the alcohol on the soldering area, let it completely evaporate, and then applying the NC flux? I'm wondering how this helps except to clean the surface off contaminants before soldering. Andy Ng Quoting Paul Edwards <[log in to unmask]>: > Always did like trichlor... > > We are currently using an EnviroSense's Enviro Gold #816 solution in > a batch cleaner to remove most NC fluxes then send the PCA through > a normal aqueous clean to remove all other residues...This works > really well... > > To make the NC flux easier to remove we normally put alcohol on > soldering area before soldering with NC flux... > > I agree with the water wash because it is an inexpensive solute and > you actually are trying to remove the residues from the surface of > the PCA not just moving them around on the surface... > > The really interesting thing is that I have never seen any water or > solvent washed commercial/industrial/consumer PCAs from Asia in at > least 15 years... > Are there any manufacturing plants in Asia using full PCA cleaning > as part of the standard assembly process? > > > Paul > > Paul Edwards > Surface Art Engineering > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting > Sent: Wednesday, December 17, 2008 5:42 AM > To: [log in to unmask] > Subject: Re: [TN] flux and board cleaning issues > > I've been experimenting with Kyzen Cybersolv(r) 141-R for removing > flux residue. So far it works far better than alcohol and > evaporates quickly. Kind of like the old 1.1.1 trich I used in my > formative years. > > Yes, we've always used alcohol too, but it really does a lousy job > of cleaning. It does a better job of diluting the flux and making > sure it then covers everything. > > My preferred choice is water soluble (OA) fluxes with a good DI > water wash when the assembly methods allow. > > Phil Nutting > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman > Sent: Wednesday, December 17, 2008 8:15 AM > To: [log in to unmask] > Subject: Re: [TN] flux and board cleaning issues > > Have you considered using some Microcare products? They may be more > effective in removing flux via hand cleaning than IPA. Compressed > air can be used, but it represents an ESD problem unless you are > using a nozzle that is grounded. > > It has been my experience that IPA would dilute the flux residues > but not necessarily remove them. It also depends on the time between > soldering and cleaning. The shorter the time, the easier it is to > remove the flux. > > Lee Whiteman, PMP > Senior Member Engineering Staff > L-3 Communications East > Telephone: (856) 338-3508 > FAX: (856) 338-2906 > E-Mail: [log in to unmask] > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob > Sent: Tuesday, December 16, 2008 7:12 PM > To: [log in to unmask] > Subject: Re: [TN] flux and board cleaning issues > > Rosin Mildly Activated > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak > Sent: Tuesday, December 16, 2008 4:04 PM > To: [log in to unmask] > Subject: Re: [TN] flux and board cleaning issues > > Bob: Why not advise on the type of flux you are using. > > Rudy Sedlak > RD Chemical Company > > --- On Tue, 12/16/08, Wilson, Bob <[log in to unmask]> wrote: > From: Wilson, Bob <[log in to unmask]> > Subject: [TN] flux and board cleaning issues > To: [log in to unmask] > Date: Tuesday, December 16, 2008, 3:55 PM > > Hi, > > I have a lead who is an IPC J-STD-001 certified trainer and she is very > good. We are using a board assembly that has a nut plate under a > high-density 26-pin DSUB. > > The girls were soaking the assemblies in an alcohol bath and the lead > assembler said she didn't want the boards soaked in alcohol because it > isn't 100% guaranteed to remove all the flux from under the connector or > nut plate. > > She has the girls trying to get a brush under there to get the flux out. > > Am I nuts or have I been under the wrong impression that alcohol and > compressed air is the best way to clean a fluxed board? I hate the idea > of me saying something like, "But...but that's the way we've > always done > it!" > > (I don't have J-STD-001 here on the design side). > > Thanks a bunch. > > Bob Wilson > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for > additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > > > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > Note: All the information contained in this e-mail and its > attachments is proprietary to Kaiser Systems, Inc. and it may not be > reproduced without the prior written permission of sender. If you > have received this email in error, please immediately return it to > sender and delete the copy you received. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > ============================================================================== > > This email and any attachments thereto may contain private, confidential, and > privileged material for the sole use of the intended recipient. Any > review, copying, > or distribution of this email (or any attachments thereto) by others > is strictly prohibited. > If you are not the intended recipient, please contact > [log in to unmask] > immediately and permanently delete the original and any copies of > this email and > any attachments thereto. > > ============================================================================== > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ============================================================================== This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited. If you are not the intended recipient, please contact [log in to unmask] immediately and permanently delete the original and any copies of this email and any attachments thereto. ============================================================================== --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------