In a message dated 11/10/08 16:56:28, [log in to unmask] writes: > Werner > > This is great news. > > Any progress in high cycle fatigue for Lead Free? > > Which of the three Las Vegas workshop will address the new creep fatigue > model in the most detail? > > Hi Scott, Pb-Free Soldering Processes: Survival, Quality, Reliability: The PROBLEMS and Pb-Free Soldering Processes: Survival, Quality, Reliability: The SOLUTIONS are really one continuous tutorial broken into 2 pieces to accommodate IPC's peculiar needs. These are the workshops where the SAC creep-fatigue model will be discussed. Werner Future workshops: Pb-Free Soldering Processes: Survival, Quality, Reliability—The PROBLEMS, December 8, Dallas, Texas Pb-Free Soldering Processes: Survival, Quality, Reliability—The SOLUTIONS, December 8, Dallas, Texas Solder Joint Reliability: Part 1—Solder Joint Reliability Fundamentals, March 29, Las Vegas Pb-Free Soldering Processes: Survival, Quality, Reliability: The PROBLEMS, March 30, Las Vegas Pb-Free Soldering Processes: Survival, Quality, Reliability: The SOLUTIONS, March 30, Las Vegas > Scott Newland > ************** AOL Search: Your one stop for directions, recipes and all other Holiday needs. Search Now. (http://pr.atwola.com/promoclk/100000075x1212792382x1200798498/aol?redir=http://searchblog.aol.com/2008/11/04/happy-holidays-from -aol-search/?ncid=emlcntussear00000001) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------