Ben Here is a chart showing DuPont's listing of Ag based conductors. I am making no advertisement for DuPont in particular - it just happened to be convenient. Heraeus and others also make thick film inks. You will see on the chart that fritted and mixed bonded systems are available. A mixed bonded system is a combo of fritted [glass] and chemical [much less glass]. There are pros and cons to each. Generically, they are all fired at 850-925°C with the fully chemically bonded systems sometimes 'liking' the higher temps. http://www2.dupont.com/MCM/en_US/PDF/selectorguides/AgConductors_selectorGuide.pdf Again, this stuff has been around for ages and I doubt you will have any problems. See what other responses you get. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben Sent: Tuesday, November 18, 2008 10:39 AM To: [log in to unmask] Subject: [TN] AgPdPt-glass frit? Technetters, Anyone heard of a silver-palladium-platinum-glass frit finish on a component? (See http://www.coilcraft.com/1008ls.cfm ) Do the same issues with Ag and AgPd finishes apply? Should I be concerned about using this in a SnPb process? Ben --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------