Hi Mike, Given that SAC+Bi solders outperform SAC, I assumed, it sounds like incorrectly, that there would be a reduction in modulus of elasticity. Werner -----Original Message----- From: Mike Fenner <[log in to unmask]> To: [log in to unmask] Sent: Fri, 14 Nov 2008 9:10 am Subject: RE: [TN] BGA Pad Cratering - PbFree Werner Generally I would not regard Bi based alloys as soft/ductile, do you have a specific one in mind? Bi has all the same properties as a ginger biscuit [except it doesn't go soggy if dunked in your tea]. Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /* Sent: Thursday, November 13, 2008 4:16 PM To: [log in to unmask] Subject: Re: [TN] BGA Pad Cratering - PbFree Hi Glenn, Indeed, there are solution options. First, easiest and most obvious, reduce cooling rate from reflow to 1.5°C/sec or less; Second, use high STII-value (Tg, Td, TE) PCB base materials, however be careful, some of these materials are more brittle; Third, use softer solder alloys (Bi, In); And fourth, to be facetious, use SnPb solders. Werner -----Original Message----- From: Glenn Torrance (gtorranc) <[log in to unmask]> To: [log in to unmask] Sent: Thu, 13 Nov 2008 9:00 am Subject: [TN] BGA Pad Cratering - PbFree Hi, Anyone have any luck in mitigating Pad Cratering in the BGAs in a Pbfree process ? I heard enlarging pads might be a consideration. Thanks in advan ce, Glenn --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ***This email, its content, and any files transmitted with i t, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.*** --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------