The EMPF Camp had a DOE for stencil printing. Measuring solder paste deposits was a problem. There are better tools now. Cpk is a problem when your process output is measured with attributes data. There is a nice discussion of this in Statistical Process Control for Surface Mount Technology by William Messina. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of john queen Sent: Tuesday, October 28, 2008 6:55 AM To: [log in to unmask] Subject: [TN] CPK Guys I am trying to make up some tools for measuring cpk of Reflow oven profiles, I am also trying to put together a DOE for screen printing. I was hoping you can all point me in the right direction or if any of you have done anything like this before. Many Thanks John --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------