The pin hole section you sited applies to wave soldered connections, as does much of the entire Section 5. Study the second paragraph on page 5-1. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Charming Chan Sent: Monday, October 20, 2008 4:54 AM To: [log in to unmask] Subject: [TN] Acceptance spec for pin hole/blow hole Hello TechNet specialist, On section 5.2.2 of spec IPC-610D, the pin hole/blow hole defect spec for class 2, 3 is 'Solder connections where pinholes, blowholes, voids, etc. reduce the connections below minimum requirements(not shown)'. My question is, what's the minimum requirements for solder joints of wave soldering? Thanks a lot. Best Regards Charming Chan PCBA Engineer -------------------------------------------------------- ZTE Information Security Notice: The information contained in this mail is solely property of the sender's organization. This mail communication is confidential. Recipients named above are obligated to maintain secrecy and are not permitted to disclose the contents of this communication to others. This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the originator of the message. Any views expressed in this message are those of the individual sender. This message has been scanned for viruses and Spam by ZTE Anti-Spam system. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------