Hey guys, thanks to all for the tips - I'll be a while following them up but I'm sure I can find the right gear based on these recommendations. regards, - Graham -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins Sent: Thursday, September 04, 2008 11:35 AM To: [log in to unmask] Subject: [TN] Wire Harness question - soldering 0 AWG wire? Hello TechNet I've been dragged (kicking and screaming) out of my comfort zone, and am looking at a wire harness. I've got some 0 awg wire to solder into a connector. We haven't tried it, but I really doubt that my Metcal MX-500 system is up to this task. Do any of you have experience with this, and if so can you recommend equipment or technique? regards, Graham Collins Halifax Production Engineering (902) 873-2000 ext. 6215 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------