Hmm! I thought HCFC-141b was forbidden in the EU??? If it is pure, then I can easily understand your problem. It will not be a good solvent for flux residues as it is hopeless for ionic components. It will dissolve the rosin (even so, not very well) and leave some of the activators behind. At the same time, I would not guarantee that there would not be a light attack of the polyimide resin itself. Or do you have a blend? Nylon is a polyamide and I've never seen a PCB made of nylon!!! Brian Juan T. Marugán wrote: > Brian, > > The solder paste we are using is a ROL0 and the cleaning solven is 141-b. > > We agree with you that something is preventing the adhesion. And about your > interesting theory, can you tell us how to "see" the invisible flux residues? > > PD. Correct. It is polyimide, not polyamide. > > Juan > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------