Dunno understand w u need calibrate. U have balls as reference, don't you? Inge ----- Original Message ----- From: "fabrice pires" <[log in to unmask]> To: <[log in to unmask]> Sent: Tuesday, September 09, 2008 7:50 AM Subject: [TN] precise void size measurement > Hi Techneters, > > I would like your advices on the best way to calibrate XRay pictures in > aim to measure precisely voids inside BGA balls, after assembly. > Everyone should agree on the fact slight setup variation on XR equipment > could change significantly the void size results. > > Do you have any trick to improve precision measures whatever the XR > equipment? > Does the use of any reference/calibration on boards exists in that aim? > > Fabrice > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------