I would not recommend any conformal coating that is spray deposit but I would consider pyraline coating process after installation. Repeated flexing will cause cracking and peeling off from the Kapton. Also may consider some type of surface prep to rough up the flex material to enhance the bond strength. Thank you, Jim Mahoney Quick Turn Flex Circuits, LLC Applications Project Manager P# 603-821-6571 F# 603-821-5723 M# 603-305-6250 ** This email and all attachments have been scanned prior to being sent** Confidentiality Notice: This page and any accompanying documents contain information that is confidential, privileged or exempt from disclosure and is intended for the exclusive use of the addressee. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution or use of the contents of this information in any manner is strictly prohibited. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Roberts, Jon Sent: Wednesday, September 03, 2008 5:42 PM To: [log in to unmask] Subject: [TN] FLEX CIRCUIT AND CONFORMAL COATING Does anyone know what IPC spec that addresses if flex circuit between two rigid boards can or cannot have conformal coating? I found Design spec IPC 2223 that addresses in paragraph 4.4 that it generally should be free of conformal coating due to make it stiff or debonding of the coating. Not sure what coating that is referring. Any ideas, thanks in advance, Jon This communication is intended only for use by the addressee(s) named herein and may contain business confidential and/or legally privileged information. If you are not the intended recipient of this e-mail, you are hereby notified that any dissemination, distribution, disclosure or copying of this e-mail and its contents is strictly prohibited. If you have received this e-mail in error, kindly notify the sender by replying to this message. In addition, please permanently delete the message and any attachments without copying or disclosing the contents. Thank you for your cooperation. THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR DEPARTMENT OF COMMERCE. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------