Yes, it could. But, so could flux residue. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of James Verrette Sent: Friday, September 19, 2008 4:23 PM To: [log in to unmask] Subject: [TN] Can desoldering and soldering fix a leaky MLCC I had a case where I was measuring about 100k accross two nets on a PCB Assembly with an Ohm meter. I removed a .1uF X7R MLCC SMT 0402 size from the board and the 100k short went away. I measured the cap and the ohm meter and the resistance was OL. I put the capacitor back on the board and remeasured the resistance and there was no short. I looked for obvious damage on the cap under a microscope, but didn't see anything. Is it possible that desoldering and resoldering by hand could cause a leaky MLCC to stop leaking? I am trying to find an explaination for what made the 100k short circuit go away. The only other expaination is that there was something under the part that caused leakaget. The boards are assembled with no-clean flux, SnPb solder paste. Based on what I have read flex cracks could cause the leakage we saw before the modification, but could desoldering and soldering cause it to go away? Jim Verrette Senior Electrical Engineer --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------