可以烘烤啦。。。。只是效果不理想。。。有很多dry solder. From: TGAsia [mailto:[log in to unmask]] On Behalf Of Cony Su Sent: 27 August 2008 11:25 To: [log in to unmask] Subject: Re: [TGA] PCB silksreen issue OSP PCB 不能烘烤的 Best Regards Cony Su _____ From: TGAsia [mailto:[log in to unmask]] On Behalf Of Roger Liu Sent: Wednesday, August 27, 2008 11:18 AM To: [log in to unmask] Subject: Re: [TGA] PCB silksreen issue Team, We bake the OSP PCB board, but the color was changed. Who can help what the problem happened? Can we still use them as normal? Best Regards! Roger Liu Office: (086) 022-25293662 Cellular:(086) 138-2098-7845