Whoa Ingemar, Are you just coming out of hibernation?? Kinda behind in your e-mails maybe??? :-) Let me check with March to see if they have some concise learning tools out there. Their site http://www.marchplasma.com/index.html did not have anything that just jumped out and grabbed me with a wealth of obvious info in the Support section, but there were multiple topics that had internal links to published papers, etc. Will just take a bit of time to muddle through them. For the most part, it is all relatively straight forward. You have Time, RF Power, Gas species, and Chamber pressure [vacuum] to play with. My simple way of thinking of it is that greater pressure means more gas atoms, therefore, with the correct amount of RF energy, I could be cleaning more aggressively - or I could be re-depositing it just as quickly..... Doing a wetting angle test on the specimen is the best litmus test one can do. Even just putting a drop of water on a part [with a control] can provide insight if a wetting angle tester is not convenient. We have multiple AP-1000's and Flextraks. Have been in communications with March of late anyway. Let me check with them to see if they have any Plasma Cleaning for Beginners documents out there. If they come back with some papers, maybe we can get Steve to put them on his 'wall' for all to see. Steve - still flying -----Original Message----- From: Hernefjord Ingemar [mailto:[log in to unmask]] Sent: Monday, August 11, 2008 7:05 AM To: TechNet E-Mail Forum; Creswick, Steven Subject: RE: [TN] Plasma Surface Treatment For Conformal Coat Trikeman, late reaction...I agree with Watt you say. One problem here: most of us know too little about running these machines. Do you know about any good books to place in the hands of our technischzans? Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven Sent: den 6 februari 2007 20:37 To: [log in to unmask] Subject: Re: [TN] Plasma Surface Treatment For Conformal Coat Joe, From a microelectronics standpoint [hermetic type of stuff] I have always been under the impression that removal of silicone residue with standard gases such as Argon, Oxygen, Nitrogen, or Argon+Hydrogen mixes was not reasonably possible - talking RF plasmas in a partially evacuated chamber, here. Our best plan, was not to have it [silicone] there in the first place - silicones have a really nasty tendency to migrate all over the place, on occasion. The greatest part of my fear of placing a silicone containing part within the chamber is that some of what gets dislodged from the piece in question may deposit on the chamber walls [instead of getting sucked out the vacuum]. This can mean that the next part to go into the chamber may get a smattering of this as it becomes knocked from the chamber walls. This would not be good for a part which was going to be wire bonded, for example. At our power levels, angstoms, or atomic layers, of contaminates are removed. I don't normally attempt to remove visibly thick layers of contaminates with the plasma because doing so usually either takes a long, long, time and/or the parts become hot and/or discolored [eg O2 will turn silver black. Go long enough and SnPb solder will get dark and dull looking, etc.]. A 'quicky' O2 plasma - say 5 minutes, at 150W, at about 150-200 mT will do a nice job of activating the surface of many plastics for promotion of adhesive adhesion though. I have little doubt that it would also improve the wetting characteristics of your bare laminate and/or solder mask, but I would not necessarily lay claim that it would remove gobs of organics [within a reasonable time frame, that is]. I'm interested in hearing what Yoda Ingemar and D Hillman have to say on the matter. PS - Ingemar, I had -16F, outside air temp this morning [-14F yesterday]. Getting more like your neck of the woods each day! Have had enough, thank-you. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US SSA) Sent: Tuesday, February 06, 2007 11:23 AM To: [log in to unmask] Subject: [TN] Plasma Surface Treatment For Conformal Coat While we're on the subject of CC, does anybody use plasma to remove stubborn organic residues (e.g. silicones) from board surfaces, or otherwise change the surface energy to promote coating adhesion? We're not talking about long or aggressive exposure here, just enough to remove a thin layer of contaminant, or roughen the surface of a glossy soldermask. So I'm not much concerned about removing markings or anything, but are there any other potential pitfalls? Joe Kane BAE Systems Johnson City, NY --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------