Interesting question. Are any of the chemistry players producing B nickel for PCB apps? Haven't come across it myself, but for info the typical B content of electroless Ni is lower than you would find in P types, typically low B plating is <3% and high B 3-6% Regards Ian Fox Lead Materials and Process engineer Goodrich ECS York Road Hall Green Birmingham B28 8LN United Kingdom Tel: +44 (0)121 607 3763 Fax: +44 (0)121 607 3658 E-mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman Sent: 27 August 2008 13:23 To: [log in to unmask] Subject: [TN] ENIG & BORON Need to get educated on this one... Was reading IPC-4552 and read that Boron and Phosphorus were used as reducing agents. I know that too much Phosphorus (> 7%) can lead to "Black Pad". Does Boron have the same effect as Phosphorus? If so, what is the UCL for Boron in the ENIG process? Just curious... Thanks. Lee Whiteman, PMP Senior Member Engineering Staff L-3 Communications East Telephone: (856) 338-3508 FAX: (856) 338-2906 E-Mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- -------------------------------------------------------------------------- Goodrich Control Systems Limited. Registered Office: Stratford Road, Solihull, West Midlands, B90 4LA. Registered in England No. 04482312. -------------------------------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------