Hi all! I'm looking for a pair of gloves that will stand-up to use in our wave solder area. We need something that will protect the operator from heat (we do a lot of selective pallets here, and they are pretty hot coming off the wave), and will stand-up to the flux. I thought I had just bought a good pair from Lab Safety Supply, but they only lasted a couple weeks before deteriorating... Anybody know of some good ones? Steve --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------