How about a hanging blacklight? I bought some standard sized bulbs to fit a shop fluorescent light fixture a while back. They used to be readily available at your neighborhood big box home improvement store. You could hang it in a vented fume hood in an isolated area to cure and vent any fumes. Or you could get your hands on a tanning bed and provide tanning as an employee perk when you're not curing your coating waste! Eric Kalgren Electrical Engineer The Ferrite Co. Inc. 165 Ledge Street Nashua, NH 03060 Phone 603-881-5234 Fax 603-881-5406 PRIVILEGED AND CONFIDENTIAL COMMUNICATION This E-mail is covered by the Electronic Communications Privacy Act, 18 U. S. C." 2510-2521 and is legally privileged. The information contained herein is confidential and is intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this transmission in error, please immediately notify the sender by telephone or via e-mail and delete the original transmission including any attachments without reading or saving in any manner. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349) Sent: Wednesday, July 02, 2008 1:11 PM To: [log in to unmask] Subject: Re: [TN] Conformal Coating Waste Yes, Same here in upstate NY (maybe not so much right now).......I would end up with a bunch of snow on them 5 months from now! Amol -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist Sent: Wednesday, July 02, 2008 11:23 AM To: [log in to unmask] Subject: Re: [TN] Conformal Coating Waste Hi Amol, We don't use UV coating so it's not an issue but I was wondering if you could put the paper out in the sun for a little bit. Of course here in Western Washington that would be a problem since we never get any sun ;-) KennyB -----Original Message----- From: Kane, Amol (349) [mailto:[log in to unmask]] Sent: Wednesday, July 02, 2008 6:17 AM To: [log in to unmask] Subject: [TN] Conformal Coating Waste Dear Technetters, We regularly use absorbent paper to rest the boards in the conformal coating booth as we spray them (UV cure coatings). A question came up recently about the paper being hazardous waste due to uncured coating on it. I want to know if: 1. Anybody else is using a similar method to coat the boards and how is disposal being handled 2. Is there an alternative to using paper in the coating booth. The disposal issue will still remain I do not want to put the paper in the UV oven for curing. Any advice will be greatly appreciated. Thanks, Amol --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- WARNING: Export Control This document may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such data by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited. CONFIDENTIALITY NOTICE: This e-mail, and any attachments, is for the sole use of the intended recipient(s) and may contain information that is confidential and protected from disclosure under the law. Any unauthorized review, use, disclosure, or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail, and delete/destroy all copies of the original message and attachments. Thank you. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------