Ioan, Unfortunately long term reliability will not be one of the wishes granted. John > That's the genie in the cap. When it bulges, you are granted 3 wishes. > > -----Message d'origine----- > De : TechNet [mailto:[log in to unmask]] De la part de Stadem, Richard D. > Envoyé : July 22, 2008 1:54 PM > À : [log in to unmask] > Objet : Re: [TN] RE: Bulging Cap > > Yes. This is how the problem manifest itself, with a bulge on the top of > the cap. However, we did not have the contamination shown just to the > left of the coil! :-) > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory > Sent: Tuesday, July 22, 2008 12:17 PM > To: [log in to unmask] > Subject: [TN] RE: Bulging Cap > > Hi Ioan! > > I'm doing fine. Staying busy trying to get back into the swing of things > at work after being gone for three-weeks. We're also getting our > Select-X installed on our new wave machine today, so I'm sure I'll be > tied-up this afternoon learning how to use it. > > Anyways, I have your picture posted. It's here: > > http://stevezeva.homestead.com/files/Bulging_Electrolytics.jpg > > Steve > > ________________________________ > > From: Ioan Tempea [mailto:[log in to unmask]] > Sent: Tuesday, July 22, 2008 10:50 AM > To: Steve Gregory > Subject: Bulging Cap > > > > Hi Steve, > > > > How are you? I hope everything is well! > > > > I have asked a question on Technet about the Panasonic caps and I think > it would be a good idea to refer to the attached picture that shows the > bulging at the top of the parts. I wonder if this is acceptable or not. > > > > Could you please post the image on your site? > > > > Thanks, > > > > Ioan > > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------