Doug, Yes, I know. It is sold under their cleaner category. Phil ________________________________ From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, July 22, 2008 12:51 PM To: TechNet E-Mail Forum; Phil Nutting Subject: Re: [TN] Washing dirty conformally coated boards Phil, That's not a cleaner, that's a stripper. n-methyl pyrrolidone (NMP) is the active stripper in many of the "environmentally friendly" coating strippers. Glycol methyl ethers too. Doug Pauls Phil Nutting <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 07/22/2008 11:24 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Phil Nutting <[log in to unmask]> To [log in to unmask] cc Subject Re: [TN] Washing dirty conformally coated boards Brian, From the manufacturer's MSDS for their recommended immersion cleaner: SECTION 2: COMPOSITION/INFORMATION ON INGREDIENTS Chemical Name CAS No. Wt. % Range 3-methoxy-3-methyl Butanol 56539-66-3 25.0-75.0 Dipropylene glycol methyl ether 34590-94-8 25.0-75.0 N-Methyl pyrrolidone 872-50-4 5.0-25.0 2-Butoxy ethanol 111-76-2 0.1-10.0 Phil -----Original Message----- From: Brian Ellis [mailto:[log in to unmask]] Sent: Tuesday, July 22, 2008 12:00 PM To: TechNet E-Mail Forum; Phil Nutting Subject: Re: [TN] Washing dirty conformally coated boards I would remove the coating with a mild solvent, such as a HCFC/HFC/HFE blend, preferably in a vapour phase machine and recoat. Brian Phil Nutting wrote: > Good morning, > > We have some circuit boards that we coat with Chemtronics Konform AR, that when returned from the field need to be washed to remove the graphite/carbon and brass dust (it won't blow off). Washing and rinsing at temperature tends to peel the conformal coating off. The currently process is hand washing and rinsing, but it is a totally uncontrolled process. > > I'm looking for recommendations for a more controlled process that is less likely to remove the coating. I just want to get the dusty stuff off the board. It looks I'm going to have to create a machine or controlled process the works at room temperature. > > Phil > > Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ________________________________ Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------