Bob, I think it might helpful to view this situation as if the parts were 2 halves of a connector. In that case, you would mask the sockets and the leads and coat most everything else. That's the way I'd leave it. I wouldn't get too hung up about the exposed metal within the actual socket. I would view the risk of having later failures from "incomplete" coverage as being fairly low. At least, compared with a connector, you don't have wicking surfaces that can trap and concentrate contaminates between conductors. Gregg -----Original Message----- From: Wilson, Bob [mailto:[log in to unmask]] Sent: Friday, July 18, 2008 10:48 AM To: [log in to unmask] Subject: [TN] conformal coating Hi! We're having a discussion about conformal coating. Does anyone have any data about acrylic coating of an EEPROM after the programmed chip is placed in the socket? Does the coating cause any problems? Is it a standard practice to mask the socket, coat the board, install the chip and then coat over the chip? Thanks a bunch. And happy Friday!! Oil prices have fallen lately. We include this news for the benefit of gas stations, which otherwise wouldn't learn of it for six months. ~William D. Tammeus Bob Wilson E/M Designer, CID+ SpectraSensors, Inc. 11027 Arrow Route Rancho Cucamonga, CA 91730 (909) 948-4110 www.spectrasensors.com www.ipc.org --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------