We are a contract manufacturer and most of our customers prefer that this is not coated. If it is a socketed chip, most will remove this item at some time in its life for a software update, test chips, etc... We have had customers in the past who have asked us to coat and we have had some big problems at test. In this scenario, it was humiseal 1C51, wich is a silicone based coating. Once the coating covered the contacts, their was no more electrical connection. Another of our customers uses a Base Chemistry of Modified Acrylic Resin that was UV curable. It was a nightmare when we had fall out. We ended up talking them into removing the socket. Hope that helps and all the best. On Fri, Jul 18, 2008 at 12:48 PM, Wilson, Bob <[log in to unmask]> wrote: > Hi! > > We're having a discussion about conformal coating. > > Does anyone have any data about acrylic coating of an EEPROM after the > programmed chip is placed in the socket? > > Does the coating cause any problems? Is it a standard practice to mask > the socket, coat the board, install the chip and then coat over the > chip? > > Thanks a bunch. > > And happy Friday!! > > Oil prices have fallen lately. We include this news for the benefit of > gas stations, which otherwise wouldn't learn of it for six months. > ~William D. Tammeus > > Bob Wilson > E/M Designer, CID+ > SpectraSensors, Inc. > 11027 Arrow Route > Rancho Cucamonga, CA 91730 > (909) 948-4110 > www.spectrasensors.com > www.ipc.org > > > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at > [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------