Hi Vladimir, You write: "That is obviously your choice but I'd prefer to stick with mine :-)"—but I have not seen your succinct definition. You write: "Be careful with using/interpreting EDS for fracture surfaces. It's NOT that straight forward. EDS cannot be used to do it. There are several reasons and the major ones are depth of penetration and the surface topography." In the meantime I got the following input: "Given that the regions of phosphorus enrichment that are typically reported at ENIG interfaces are in the range of 50 - 100 Angstroms, and that, at typical accelerating voltages, EDS sampling depths are in the 1000+ Angstrom range, EDS measurements would be of bulk deposit composition, not interfacial." Is this what you were telling me? Werner ************** Gas prices getting you down? Search AOL Autos for fuel-efficient used cars. (http://autos.aol.com/used?ncid=aolaut00050000000007) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------