If you solder components by hand with 320dC, you also solder lead free with 320dC. Otherwise you can thermally damage the component or the adhesion of solder lands from the board. Rule of thump: manual solder time is maximum 5 seconds, the solder have to be liquid for at least 3 seconds before it solidifies.. If you cannot solder within this window, increase the thermal mass of the solder tip. NEVER increase the iron tip temperature. Success! Peer Langeveld Consultant Soft Soldering Processes 5502 VH 8 NL 2008/6/26 Luan Nguyen <[log in to unmask]>: > Dear All, > We have a question about set temperature for hand soldering. We were using Hakko FM-202. > - For tin lead, we set 320 C degree > - For lead-free, we plan to set 380 C degree. However, we can not find any standard (IPC, J-STD) mention to set temperature. We refer some documents, experience sharing that temperature range is from 370 C degree to 425 C degree. Moreover, in there is also mention as "> 80 W hand soldering is always OK" that effect us due to Hakko FM-202 have power consumption of soldering iron is 70W. > > Please help me any reference, any document, any advice. > > Thanks and best regards, > > > *************************** > Nguyen Hoang Luan > QC&Training Supervisor > Spartronics VietNam Co, Ltd. > No.3, Street No.6, VSIP > Th An Dist., BDuong Prov., VN > Tel: (84-650) 784 890 > Fax: (84-650) 784 891 > Mobile: 090.3.667448 > Email: [log in to unmask] > *************************** > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------