Just thinking this through and this is what I speculate/hypothesise: So far as I know you can't plate an alloy, so if they have plated then they must have co-plated the Sn Ag and Cu in the appropriate proportions for them to melt/dissolve on soldering, That might do something to the soldering process, possibly non homogenous/grainy joints, soldering process would be a little slower and need more time for homogeneity, this would lead to a reduction in tombstoning though. I doubt it would be that significant though. IF you can plate an alloy, or functional alloy, the same applies, a 95.XX pure tin coat would not be that different to normal 99.X% Most probably they have hot tinned them in SAC and used "plating" as a sort of generic coating term, not a specific. In that case there is likely to be more solder than on a plated part. The alloy would still dissolve into the molten Sn/Pb (just as pure tin MP 232C does) as normal. Being hot dipped the solder joint is already made so wetting would be OK, and joint formation correspondingly quicker. Add in: The MP of SAC at 217C could be well below peak profile, so now we have a raised Surface tension mix (from the added high Sn content of SAC) in a fast joint formation: a recipe for the tombstoning observed by Geert. Regards Mike Fenner Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Pb-free: www.Pb-Free.com --------------------- Indium Corporation Incorporated in New York, USA Registered office: (Not for correspondence) 77-97 Harpur Street, Bedford , UK Registered number: fc16473 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David Fischer Sent: Monday, June 23, 2008 3:41 AM To: [log in to unmask] Subject: Re: [TN] SAC Plated Passives with SnPb Solder Paste These are precision resistors definitely plated with SAC305 - ... it's in the suppliers spec and in their part numbers, and we have talked with them about it. Good feedback so far, thanks everyone. If there is more feedback, I'd appreciate it. Regards, David Fischer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David Fischer Sent: Friday, June 20, 2008 6:18 PM To: [log in to unmask] Subject: [TN] SAC Plated Passives with SnPb Solder Paste Good Day, I am aware of the nuances of mixing SAC solder ball BGA's with SnPb solder paste, but are there any concerns, cautions or steps to take when soldering SAC plated passives (chip resistors, chip caps) to a PCB using SnPb solder paste? Thanks, David Fischer Manufacturing Engineering Manager ATEOps NPI Teradyne, Inc ***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.*** --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------