Werner, What about my question makes you conclude that underfill is not needed? Because I implied that the part is small by description of the solder bump? Why do you discount the need for underfill on small parts so easily? There will be some stress induced in the solder joints due to CTE mismatch, and although the strain in a small part will be exponentially less than in a larger part, if the size and quantity of the solder bumps are not enough to withstand the stress, then they will fail. I am no expert on flip chip - are there industry standard designs that ensure smaller chips will not need underfill? Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /* Sent: Thursday, June 05, 2008 3:36 PM To: [log in to unmask] Subject: Re: [TN] Chip on Board and Solder Mask Hi Ben, For the components for which the question was posed, you do not need underfill. Underfill have the function to put the solder joints of larger components under compression, thereby imcresing fatigue life as well as not showing functional failures even if SJs are fractured. Werner Future workshops: Reliability Issues with Lead-Free Soldering Processes, June 17, London Interconnect Failures and Design for Reliability for PCB PTHs, June 17, London Solder Joint Reliability: Parts 1 through 4, July 17/18, Thal, Switzerland Pb-Free Soldering Processes-Survival, Quality, Reliability, August 18, Orlando Reliability Issues with Lead-Free Soldering Processes, September 22, Schaumburg Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, ENIG), September 22, Schaumburg ************** Get trade secrets for amazing burgers. Watch "Cooking with Tyler Florence" on AOL Food. (http://food.aol.com/tyler-florence?video=4?& NCID=aolfod00030000000002) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------