Brian is exactly correct. But you must remember if you are not RINSING the saponifier correctly you are not removing the flux as well. The flux will add to the level of corrosive and hygroscopic residue. If saponifier is left on it will be a easy removed if water can get to the area. We find with QFN and other low standoff devices that flux, saponifier and water are left under these components and they cause performance problems such as leakage, and dendrite growth. Many of today saponifiers are not as difficult to clean as the original terpene D-limonene cleaners would take multiple rinses to completely remove the material. The residue left after cleaning if not properly rinsed with clean water can cause leakage and corrosion problems. Terry Munson Foresite 765-457-8095 In a message dated 5/6/2008 2:08:55 A.M. Eastern Daylight Time, [log in to unmask] writes: I would say you have a problem. Saponifier usually has, inter alia, two components, an amine and a surfactant. The amine, commonly monoethanolamine, is ionic and the surfactant is commonly an ethylene glycol or similar. The latter has a low vapour pressure and is hygroscopic (and this generally applies to all surfactants, even if the chemistry family is different. It can also form a matrix which can hold the amine in suspension, slowing down iôts evaporation. The idea of leaving hygroscopic residues is anathema to me. If they are mixed with an ionic residue, it is double anathema. IMHO, and in my experience, saponifier cleaning MUST be followed, not by a simple rinse cycle, but by a full wash and rinse cycle, exactly as if it were a water-soluble flux. Brian - bogert wrote: > May 5, 2008 > > I have the following question: If a saponifier is used with a DI > cleaning machine to clean PWAs and the cleaning does not remove all > traces of the saponifier, is there any concern, including sugsequent > exposure, to a humid environment? Any technical reports on this subject? > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 > ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- **************Wondering what's for Dinner Tonight? Get new twists on family favorites at AOL Food. (http://food.aol.com/dinner-tonight?NCID=aolfod00030000000001) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------