What became of this issue? I have not seen any more threads of e-mail. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: Tuesday, April 29, 2008 9:59 PM To: [log in to unmask] Subject: Re: [TN] Blue Voids Are the voids in the glass bundle or between the glass bundle and the resin? If the former, you have a glass supplier problem (not all the weaving assistant burned off?)-- if the latter, then I would suspect incorrect pH in the adhesion promoter application bath. Bill Kenyon Global Centre Consulting 3336 Birmingham Drive Fort Collins, CO 80526 Tel: 970.207.9586 Cell: 970.980.6373 **************Need a new ride? Check out the largest site for U.S. used car listings at AOL Autos. (http://autos.aol.com/used?NCID=aolcmp00300000002851) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------