I think you are looking at a typo. Thieved is the word commonly used. If the solder is thieved into the via hole a connection between the part and the land may not be as strong. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard Sent: Thursday, May 08, 2008 1:34 PM To: [log in to unmask] Subject: [TN] The meaning of "skived" Can anyone define "skived" as in: IPC-A-600 2.9.3.3 Ball Grid Array (Solder Dam) "....in order to avoid solder being skived from the attachment joint into the via." Online dictionaries define skive as: to slice off (leather, rubber, etc.) in thin layers; shave. It sort of gives me an idea, but it really isn't very clear. Thanks in advance. Genny --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------