If we make the land narrower than the part and minimize the length, won't that compromise both mechanical strength and solder joint life in a thermal cycling environment? My experience with solder joint failure on chip components the joint cracks down the face and under the part. If the height of the fillet is reduced the time to failure will also reduce. No? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /* Sent: Wednesday, May 21, 2008 5:51 PM To: [log in to unmask] Subject: Re: [TN] 0402 anti-tombstoning land pattern Hi Dean, Make the land pattern narrower than the component-I know, I know, tough to do with 0402's as well as shorter thus producoing less of a fillet [which is ,of course, the root cause for the tombstoning] Werner Future workshops: Reliability Issues with Lead-Free Soldering Processes, June 17, London Interconnect Failures and Design for Reliability for PCB PTHs, June 17, London Pb-Free Soldering Processes-Survival, Quality, Reliability, August 18, Orlando Reliability Issues with Lead-Free Soldering Processes, September 22, Schaumburg Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, ENIG), September 22, Schaumburg ************** Get trade secrets for amazing burgers. Watch "Cooking with Tyler Florence" on AOL Food. (http://food.aol.com/tyler-florence?video=4& ?NCID=aolfod00030000000002) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------