Q21: add operation and test temp range are outside the commercial product , I.e. Differ significantly from the office enviroment product. Graham, excellent answer. My hats off. Jk -------------------------- Sent using BlackBerry ----- Original Message ----- From: TechNet <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Sent: Wed Apr 02 02:18:53 2008 Subject: Re: [TN] Various questions Habib As Dr Christian has already pointed out, you ask too much - you should attend our meetings to get a better understanding of the issues you raise. However, trying to be helpful, let me answer you briefly on each your questions: On 1 Apr 2008, at 15:14, SAHLI habib wrote: > Is there someone who wants to answer my questions? > > Best regards. > ----- Original Message ----- > From: SAHLI habib > To: [log in to unmask] > Sent: Thursday, March 20, 2008 1:01 PM > Subject: Various questions > > > Dear Technetters, > > Can I have the privelege to get brief answers to all my following > questions : > > 1- Main copper thickness used in Automotive market? As thin as possible > > 2- Does Automotive market is asking for copper thickness reduction? Yes. > > 3- What is the standard maximum and minimum bow and twist for Pcbs > with BGA components? Very little. > > 4- What is the standard tolerance for press-fit PTH? Small. > > 5- When is panel plating suggested and When is pattern plating > suggested? Refer to standards. > > 6- What is the standard value for annular ring for Pcbs with high > copper thicknes (more than 3 oz)? Refer to standards. > > 7- Is AOI detecting all the PCB defects? No. > What defects are not detected? Those that are not detectable by AOI method > > 8- Is the automotive market requesting 100% AOI in internal and > external layers? Maybe. > > 9- What the is the maximum offset between copper and solder mask > requested in the automotive market? Refer to standards. > > 10- What the is the maximum offset between copper,solder mask and > holes requested in the automotive market? Refer to standards. > > 11- What is the main surface finish for Automotive? OSP - ENIG - HASL - ImSn - it depends on the application. > > 12- What product application is used OSP for? It depends > > 13- What product application is used ENIG for? It depends > > 14- What product application is used Immersion Silver for? It depends > > 15- Is Screen printing in use for Automotive market? Probably > > 16- Is Screen printing used to mark code matrix? Sometimes > > 17- What is the maximum accepted value of Ionic contamination in > Automotive market. (µg Na Cl/square for inch) Often <0.2mg/cm2 NaCl equivalence > > 18- Are customers requesting Ioni chromatography or any other > similar analysis? Yes. > > 19- Is the automotive market requesting PEA packaging (Electrostatic > Protected Area)? Usually. > > 20- Is Pollution gas test required for Automotive market? Yes but not always. > > 21- What are the Significant Characteristics defined by Automotive > market? High reliability. > > 22- What are the main characteristics for satndard FR4 base material? Flame retardance. > > 23- What are the main characteristics for lead free base material? ? > > > Thank you in advance for your support. > > Habib > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask] > : SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask] > : SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] > or 847-615-7100 ext.2815 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------