I was able to unzip the files but not able to view. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Willis Sent: Thursday, April 10, 2008 3:02 AM To: [log in to unmask] Subject: Re: [TN] Polymer cored solder spheres Images and sections Sorry for the delay but here are the plastic ball solder joint images in a zip file. Looking at the images I obviously have never finished grinding and polishing the sections so that is why they are not perfect, work in progress. I obviously had to stop working on this little project and move on to something else between 204 and 07? www.ASKbobwillis.com/bobwillisballs.zip David Bernard of Dage has some more of the plastic ball x-ray images and has also produced some CT images. Hope they help. Bob Willis 2 Fourth Ave, Chelmsford, Essex, CM1 4HA England Tel: (44) 1245 351502 Fax: (44) 1245 496123 Mobile: 07860 775858 www.ASKbobwillis.com Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th May www.ASKbobwillis.com/faworkshops.pdf New "Printed Board Inspection & Quality Control" 3 July www.ASKbobwillis.com/PCBworkshop.pdf --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------