I thought there was a minimum thickness in J-STD-001 that allowed you to skip the gold removal for PTH, but for surface mount gold removal was always required. Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist Sent: Wednesday, April 30, 2008 11:29 AM To: [log in to unmask] Subject: Re: [TN] IPC-J-STD-001D @ 3.9.3 GOLD REMOVAL Dave, The way I've always interpreted this is if you have a gold component lead that is 1" long and you are going to be soldering the bottom .1" of the lead into the board then .095" needs to have the gold removed. KennyB Ext 43-----Original Message----- From: David Reed [mailto:[log in to unmask]] Sent: Wednesday, April 30, 2008 7:30 AM To: [log in to unmask] Subject: [TN] IPC-J-STD-001D @ 3.9.3 GOLD REMOVAL Recently a customer asked the following question. Here is his question. I do have a question of interpretation for you regarding "gold removal". In section 3.9.3 it states that ".....95% of the surface to be solder ....." needs to have gold removed. Failing to achieve the 95% is considered a class 3 defect. We are having boards with PIH gold plated leads rejected for not meeting this requirement. Part of the problem is making the determination as to where and how the 95% is measured. Can you clarify for us exactly where the 95% is measured on the lead. Before I reply to this engineer I thought to see if you had any input. Thanks, Dave --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------