The quickest way to see if an ICT fixture is causing damage is to repeatedly test a good board to see if you can precipitate failure. Work out how many times to test from the current failure rate. Regards Rex Rex Waygood Technical Manager PartnerTech Poole Ltd Benson Road Poole Dorset BH17 0RY United Kingdom Tel: +44 (0)1202 674333 Fax: +44 (0)1202 678028 DDI: +44 (0)1202 338222 Mob: +44 (0)7887 997403 [log in to unmask] www.PartnerTech.co.uk -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Chandler Sent: 29 April 2008 13:03 To: [log in to unmask] Subject: Re: [TN] Cracking Ceramic Cap Have you tried to take any strain measurements during the processing downstream of SMT? ICT fixtures can induce excessive strain as well as any other fixturing/pallets. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ------------------------------------------------------------------------------- The information contained within this e-mail and any attachments contained therein may be confidential and/or legally privileged and is for the use of the intended recipient only. If you are not the intended recipient please delete it from your system and notify the sender by return e-mail. The content of this e-mail may not be copied or disclosed to any third parties without prior permission from the sender. E-mail is susceptible to data corruption, interception, tampering and viruses. We do not accept any liability for any such incidents or any consequences thereof. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------